倾斜籽晶法控制镍基单晶高温合金晶体取向研究

YANG Shuai, BAO Jun, YANG Xiqiong, ZHENG Qiao, LIU Qian,ZHANG Jian,HU Songsong

Journal of Materials Engineering(2025)

Cited 0|Views2
Key words
Ni-based single crystal superalloy,inclined seeding,crystal orientation,solidification process