Exploring the Deformation Mechanisms and Mechanical Properties of Fused Silica Through Nanoindentation and Ramp-Nanoscratching

Wear(2025)

Cited 0|Views0
Key words
Fused silica,Hardness-yield stress correlation,Densification,Onset prediction of densification