Effects on High Content of MSWI Fly Ash for the Deterioration and Immobilization Performance of Blast Furnace Slag-Desulfurization Gypsum-Based Binder
CONSTRUCTION AND BUILDING MATERIALS(2025)
Key words
MSWI fly ash,Immobilization,Deterioration,Ettringite,Cracking,Zn2SiO4