The particle size and morphology of superalloy powders are crucial parameters that significantly influence the performance of additive manufacturing (AM) processes. This study investigates the effects of atomization pressure on these characteristics through a combination of computational fluid dynamics (CFD) simulations and vacuum induction melting gas atomization (VIGA) experiments. The CFD simulations revealed that increasing the atomization pressure from 2.0 MPa to 3.5 MPa resulted in a rise in maximum gas velocity from 526 m/s to 537 m/s and a reduction in median particle size (D50) from 60.9 mu m to 37.5 mu m. Subsequent experiments demonstrated a decrease in D50 from 52.9 mu m to 35.6 mu m, and sphericity from 0.9432 to 0.9377, as pressure increased. The particle size results of the atomization experiments and numerical simulations show strong consistency, validating the accuracy of the numerical simulation results. The volume of hollow particles also increased slightly in specific size fractions. These results suggest that higher atomization pressures produce finer powders with lower sphericity, but also promote particle adhesion, reducing the overall refinement effect. This study provides insights into optimizing atomization conditions for the precise control of superalloy powders in AM. (c) 2024 Chinese Society of Particuology and Institute of Process Engineering, Chinese Academy of Sciences. Published by Elsevier B.V. All rights are reserved, including those for text and data mining, AI
MoreTranslated text
Key words
Superalloy powders,Additive manufacturing,Atomization pressure,CFD modeling,Particle size,Morphology
求助PDF
上传PDF
View via Publisher
AI Read Science
AI Summary
AI Summary is the key point extracted automatically understanding the full text of the paper, including the background, methods, results, conclusions, icons and other key content, so that you can get the outline of the paper at a glance.
Example
Background
Key content
Introduction
Methods
Results
Related work
Fund
Key content
- Pretraining has recently greatly promoted the development of natural language processing (NLP)
- We show that M6 outperforms the baselines in multimodal downstream tasks, and the large M6 with 10 parameters can reach a better performance
- We propose a method called M6 that is able to process information of multiple modalities and perform both single-modal and cross-modal understanding and generation
- The model is scaled to large model with 10 billion parameters with sophisticated deployment, and the 10 -parameter M6-large is the largest pretrained model in Chinese
- Experimental results show that our proposed M6 outperforms the baseline in a number of downstream tasks concerning both single modality and multiple modalities We will continue the pretraining of extremely large models by increasing data to explore the limit of its performance
Upload PDF to Generate Summary
Must-Reading Tree
Example

Generate MRT to find the research sequence of this paper
Data Disclaimer
The page data are from open Internet sources, cooperative publishers and automatic analysis results through AI technology. We do not make any commitments and guarantees for the validity, accuracy, correctness, reliability, completeness and timeliness of the page data. If you have any questions, please contact us by email: report@aminer.cn
Chat Paper
Summary is being generated by the instructions you defined