Study on Surface Chemical Composition of Argon Atomized Superalloy Powder Based on TOF-SIMS

Yufeng Liu, Huaqiang Zhu, Chunlin Zhang,Lichong Zhang,Fan Xu,Liyuan Zhao, Xinyu Yang, Zhou Li,Tinglu Song,Guoqing Zhang

APPLIED SURFACE SCIENCE(2025)

Cited 0|Views11
Key words
Superalloy powder,TOF-SIMS,Surface chemical composition,Primary particle boundaries,Binding affinity