Improvement of Butt-Fusion Welding Procedure and Performance Evaluation Method for Thick-Walled Bimodal Polyethylene Pipes

Zhenchao Wang, Shijun Zhang, Jichun Qie, Qijiang You, Lu Xu,Qiuju Zhang

POLYMER TESTING(2024)

Cited 1|Views0
Key words
HDPE pipe,Butt fusion welding,Welding procedure,Welding interface,Performance testing