Microstructural Evolution of Grain Refinement in Superalloy Inconel 718 During Low Temperature and Slow Strain Rate Hot Compression
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T(2024)
关键词
Inconel 718,Grain refinement,Hot compression,Deformation,Dynamic recrystallization