Classification of Ultrasonic B-Scan Images from Welding Defects Using a Convolutional Neural Network

Hongbin Sun,Richard Jacob, Pradeep Ramuhalli

13th Nuclear Plant Instrumentation, Control &amp Human-Machine Interface Technologies (NPIC&ampHMIT 2023)(2023)

Cited 0|Views1