Oxidation-creep Interactions for an Hf-doped Ni-based Superalloy with Different Wall Thickness at 760 °C

CORROSION SCIENCE(2024)

Cited 0|Views27
Key words
Rupture,Ni-based superalloy,Recrystallization,Corrosion,Cracking,Voids