Microstructure and Deformation Workability of Ni-based Superalloy Udimet720Li Fabricated by Composite Shear Flow Casting

JOURNAL OF ALLOYS AND COMPOUNDS(2023)

Cited 1|Views18
Key words
Udemit720Li,Microstructure,Composite shear flow casting,Segregation,Crack,Stress concentration