Strain Localization and Crack Initiation Behavior of a PM Ni‐based Superalloy: SEM‐DIC Characterization and Crystal Plasticity Simulation

Fatigue & Fracture of Engineering Materials & Structures(2022)

引用 14|浏览21
关键词
crack initiation,crystal plasticity,fatigue indicator parameter,PM Ni-based superalloy,SEM-DIC