Nanoindentation Study of the Effect of Low-Temperature Ion Irradiation on the Hardness of a Ferritic–Martensitic EK-181 Steel
Russian metallurgy Metally(2019)
Key words
ferritic–martensitic steel,ion irradiation,radiation damage simulation,hardness,nanoindentation